ASTM A671 CJE115 Chav Kawm 22 Hlau Yeeb Nkab

1. ASTM A671 CJE115 Chav Kawm 22 yog dab tsi?

Txuj: Hluav taws xob-fusion-welded (EFW) carbon steel yeeb nkab rauultra-siab- kev pabcuam cryogenic(-115 ° F / -81.7 ° C).

Chav Kawm 22: Hydrostatic xeem siab ntawm22,000 psi (152 MPa)(qib siab tshaj hauv A671 tus qauv).

Tus cim tseem ceeb:

"CJE115"=Charpy V-notch impact tested at-115℃Fnrog min. 15 ft-lb (20 J).

Yuav tsum normalizationrau grain refinement.

2. Qhov twg yog nws feem ntau siv?

Heev -siab cryogenics:

LNG carrier containment systems

Ua kua hydrogen thauj pipelines

Tshwj xeeb zog:

Deepwater roj & roj risers

Arctic siab hlab ntsha

Nuclear auxiliary systems: Cryogenic coolant loops

3. Mechanical & tshuaj muaj zog?

Lub zog:

Tensile: Ntau dua lossis sib npaug rau 60 ksi (414 MPa)

Tawm tswv yim: Ntau dua lossis sib npaug rau 35 ksi (241 MPa)

Toughness:

100% cuam tshuam kuaj ntawm-115℃F

Elongation: Ntau dua lossis sib npaug li 22% (scaled ib thickness)

Chemistry:

Carbon: Tsawg dua lossis sib npaug li 0.30%

Tsawg S / P (tsawg dua lossis sib npaug rau 0.035% txhua)

4. Cov kev cai tsim khoom?

Vuam:

EFW nrog100% radiography (RT)+ UT rau tag nrho -ntev seams.

Kev sim:

Hydrostatic siab:22,000 psi(152 MPa)

Ntxiv NDE (MT/PT) rau thaj chaw tseem ceeb.

Traceability:

Thaum tshav kub kub- cov ntawv ceeb toom cuam tshuam tshwj xeeb.

5. Cov txheej txheem Fabrication?

Vuam:

Preheat: 200-400 ° F (93-204 ° C)

PWHT required for thickness >1.5 "(38mm).

Kev tsim:

Txias khoov tau tso cai (min. 5D radius).

Kev tsim kub yuav tsum tau rov ua dua- normalization.

Kho:

Sib tsoo qhov tob Tsawg dua lossis sib npaug li 10% phab ntsa thickness (ib ASTM A671 Sec.12).